Using
the internal mould as a bending template, the sides are bent on a heated
copper pipe, allowed to springback for a few hours, then bent again. I
don't wet the sides during bending to avoid distortion of the figured
maple. The sides bend easily if their thickness is correct, about 1.5
mm. Final thicknessing before bending is done with a cabinet scraper and
hand scraper
|